Effect of Cu Content on Mechanical Properties of Ultra High Strength Low Carbon Bainitic Steel
|更新时间:2026-01-21
|
Effect of Cu Content on Mechanical Properties of Ultra High Strength Low Carbon Bainitic Steel
Special SteelVol. 28, Issue 1, Pages: 19-20(2007)
作者机构:
1. 武汉科技大学高温陶瓷与耐火材料湖北省重点实验室,武汉,430081
2. 武汉钢铁集团公司,武汉,430080
作者简介:
基金信息:
DOI:
CLC:
Received:19 May 2006,
Online First:12 January 2023,
Published:12 January 2007
稿件说明:
移动端阅览
宋新莉, 郭爱民, 袁泽喜, et al. Effect of Cu Content on Mechanical Properties of Ultra High Strength Low Carbon Bainitic Steel[J]. Special Steel, 2007, 28(1): 19-20.
DOI:
宋新莉, 郭爱民, 袁泽喜, et al. Effect of Cu Content on Mechanical Properties of Ultra High Strength Low Carbon Bainitic Steel[J]. Special Steel, 2007, 28(1): 19-20.DOI:
Effect of Cu Content on Mechanical Properties of Ultra High Strength Low Carbon Bainitic Steel
0.0013~0.0023B) was melted by a 50kg vacuum induction furnace. Teat results showed that with increasing Cu content from 1.0% to2.5%
the precipitation speed of e-Cu in steel and the peak hardness increased; and with increasing Cu%
the yield strength of direct-quenching(DQ)steel after rolling increased from 865 MPa to918 MPa and the yield strength of DQ + 500 ℃ tempering steel increased from 935 MPa to1140 MPa
while the tensile strength and impact toughness of DQ+500 ℃ tempering1.0~2.5Cu steel were lower than that of DQ steel.