Physical and Mathematical Study on Flow Control Device of Tundish for 5-Strand billet Casting at Chongqing Steel
更新时间:2026-01-21
    • Physical and Mathematical Study on Flow Control Device of Tundish for 5-Strand billet Casting at Chongqing Steel

    • Special Steel   Vol. 28, Issue 1, Pages: 1-3(2007)
    • Received:03 August 2006,

      Online First:10 January 2023,

      Published:10 January 2007

    移动端阅览

  • 陈登福, 佐祥均, 郑辉, et al. Physical and Mathematical Study on Flow Control Device of Tundish for 5-Strand billet Casting at Chongqing Steel[J]. Special Steel, 2007, 28(1): 1-3. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Orthogonal Test of Water Model for Optimization of Structure of Tundish
A Study on Water Model and Numerical Simulation of Flow Field in Slab Casting Mold with Different Width
An Experiment on Water Model for Bottom Gas Blowing of a 34 t Tundish
Hydraulic Simulation of Optimization of Flow Control Devices for a Tundish of Eight-Strand Continuous Casting
A Study on Optimization of Structure of Eight-Strand Tundish for Billet Concasting

Related Author

曹雄
张胤
贾攀
韩翠珍
张大江
王翠娜
靳星
谢鑫

Related Institution

内蒙古科技大学材料与冶金学院
内蒙古科技大学稀土学院
南京钢铁股份有限公司中厚板卷厂
内蒙古科技大学:1稀土学院
内蒙古自治区白云鄂博矿多金属资源综合利用重点实验室和省部共建国家重点实验室培养基地
0