Predictive Model for End Aim Temperature of Arc Furnace Based on Hybrid Genetic Algorithm
更新时间:2026-01-21
    • Predictive Model for End Aim Temperature of Arc Furnace Based on Hybrid Genetic Algorithm

    • Special Steel   Vol. 28, Issue 5, Pages: 22-24(2007)
    • Received:05 April 2007,

      Online First:13 February 2023,

      Published:13 February 2007

    移动端阅览

  • 姜静, 李华德, 孙铁, et al. Predictive Model for End Aim Temperature of Arc Furnace Based on Hybrid Genetic Algorithm[J]. Special Steel, 2007, 28(5): 22-24. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Predictive Model for Carbon Content in Steel Grade Melting by Arc Furnace Based on Hybrid Coding Method
Temperature Prediction of GCr15 Biilet Core Based on Heating Furnace Embedded Thermocouple Experiment

Related Author

姜静
孟利东
李素玲
姜琳
韩怀宾
虞学庆
白瑞娟
王维

Related Institution

山东理工大学电气学院
安阳钢铁公司二炼厂
东北大学轧制技术及连轧自动化国家重点实验室
河南济源钢铁(集团)有限公司
河南省特殊钢材料研究院有限公司
0