Effect of Rolling Process Parameters on Structure and Properties of 0.06C-0.31Mo Microalloying High Strength Pipeline Steel
|更新时间:2026-01-21
|
Effect of Rolling Process Parameters on Structure and Properties of 0.06C-0.31Mo Microalloying High Strength Pipeline Steel
Special SteelVol. 28, Issue 1, Pages: 29-31(2007)
作者机构:
1. 太原钢铁公司,太原,030003
2. 韩国浦项工业大学,韩国,790-784
作者简介:
基金信息:
DOI:
CLC:
Received:10 July 2006,
Online First:13 January 2023,
Published:13 January 2007
稿件说明:
移动端阅览
吴晓丹, HakcheolLee, YoungMinKim, et al. Effect of Rolling Process Parameters on Structure and Properties of 0.06C-0.31Mo Microalloying High Strength Pipeline Steel[J]. Special Steel, 2007, 28(1): 29-31.
DOI:
吴晓丹, HakcheolLee, YoungMinKim, et al. Effect of Rolling Process Parameters on Structure and Properties of 0.06C-0.31Mo Microalloying High Strength Pipeline Steel[J]. Special Steel, 2007, 28(1): 29-31.DOI:
Effect of Rolling Process Parameters on Structure and Properties of 0.06C-0.31Mo Microalloying High Strength Pipeline Steel
The effect of rolling parameters such as 35.0%~52.0% reduction rate in recrystallization region
60.2% ~70.3% reduction rate in non-recrystallization region
cooling rate(20~38 ℃/s)on structure and mechanical properties of0.06C-0.31Mo V-Nb-Ti-B microalloying steel has been studied by Cleeble thermal simulation machine.The test results sbowed that with increasing cooling rate
the upper bainite volume percentage increased led to increasing strength of steel
and the more acicular ferrite content in bainite matrix the more upper shelf energy(USE)of steel and the lower ductile brit- tle transition temperature
therefore the acicular ferite in bainite matrix could improve the mechanical propertics of pipeline steel.