Structure and Galvano-Chemistry Behavior of Welded Junction of Stainless Steel 1Cr18N9Ti and 1Cr13
|更新时间:2026-01-21
|
Structure and Galvano-Chemistry Behavior of Welded Junction of Stainless Steel 1Cr18N9Ti and 1Cr13
Special SteelVol. 29, Issue 4, Pages: 60-62(2008)
作者机构:
内蒙古科技大学材料与冶金学院,包头,014010
作者简介:
基金信息:
DOI:
CLC:
Received:14 January 2008,
Online First:23 December 2022,
Published:23 December 2008
稿件说明:
移动端阅览
赵勇桃, 李文学, 赵莉萍, et al. Structure and Galvano-Chemistry Behavior of Welded Junction of Stainless Steel 1Cr18N9Ti and 1Cr13[J]. Special Steel, 2008, 29(4): 60-62.
DOI:
赵勇桃, 李文学, 赵莉萍, et al. Structure and Galvano-Chemistry Behavior of Welded Junction of Stainless Steel 1Cr18N9Ti and 1Cr13[J]. Special Steel, 2008, 29(4): 60-62.DOI:
Structure and Galvano-Chemistry Behavior of Welded Junction of Stainless Steel 1Cr18N9Ti and 1Cr13
The structure of welded junction of 1Cr18Ni9Ti austenite stainless steel plate and 1Crl3 martensite stain- less steel plate welding by 1Cr18Ni9Ti electrode has been observed and analyzed by metallographic method; and the polarization curves and alternating current impedance curves were measured by immersion test of simulation seawater solution to contrast and analyze the corrosion resistance of weld seam and parent metals. Results showed that the structure of weld junction was typical columnar solidified structure; in welded junction
the martensite parent metal and weld seam region were easy to be corroded
while the austenite parent metal was not easy to be corroded.