Effect of Recrystallizing Isothermal-Annealing on Structure and Hardness of DDQ Cold-Rolled Deep Drawing Sheet
|更新时间:2026-01-21
|
Effect of Recrystallizing Isothermal-Annealing on Structure and Hardness of DDQ Cold-Rolled Deep Drawing Sheet
Special SteelVol. 29, Issue 5, Pages: 63-64(2008)
作者机构:
1. 武汉科技大学钢铁冶金资源利用省部共建教育部重点实验室,武汉,430081
2. 涟源钢铁公司技术中心,娄底,417009
作者简介:
基金信息:
DOI:
CLC:
Received:23 March 2008,
Online First:09 January 2023,
Published:09 January 2008
稿件说明:
移动端阅览
杨奕, 徐光, 郁盛富, et al. Effect of Recrystallizing Isothermal-Annealing on Structure and Hardness of DDQ Cold-Rolled Deep Drawing Sheet[J]. Special Steel, 2008, 29(5): 63-64.
DOI:
杨奕, 徐光, 郁盛富, et al. Effect of Recrystallizing Isothermal-Annealing on Structure and Hardness of DDQ Cold-Rolled Deep Drawing Sheet[J]. Special Steel, 2008, 29(5): 63-64.DOI:
Effect of Recrystallizing Isothermal-Annealing on Structure and Hardness of DDQ Cold-Rolled Deep Drawing Sheet
试验研究了TSCR(Thin Slab Casting and Rolling)薄板坯连铸连轧工艺生产的(%)0.003C-0.05Al- 0.06Cu钢DDQ(Deep Drawable Quality)级深冲薄板的再结晶退火后的组织和HB硬度。结果表明
该钢DDQ级冷轧深冲薄板的再结晶温度为~550℃
合适的等温退火温度为650℃。
Abstract
The recrystallized annealed structure and HB hardness of DDQ(Deep Drawable Quality)cold-rolled deep drawing sheet of0.003C-0.05Al-0.06Cu steel produced by TSCR(Thin Slab Casting and Rolling)process have been test- ed and researched. Results showed that the recrystallization temperature of the DDQ cold-rolled deep drawing sheet was ~550 ℃
and the available isothermal-annealing temperature was 650 ℃.