Process Practice for W600 Non-Oriented Silicon Steel Produced by 120 t LD-RH-LF CSP Flow Sheet
更新时间:2026-01-21
    • Process Practice for W600 Non-Oriented Silicon Steel Produced by 120 t LD-RH-LF CSP Flow Sheet

    • Special Steel   Vol. 29, Issue 6, Pages: 34-36(2008)
    • Received:18 May 2008,

      Online First:07 December 2022,

      Published:07 December 2008

    移动端阅览

  • 李应江, 包燕平. Process Practice for W600 Non-Oriented Silicon Steel Produced by 120 t LD-RH-LF CSP Flow Sheet[J]. Special Steel, 2008, 29(6): 34-36. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Comparison of Cleanliness of Pipeline Steel Refining by RH-LF and LF-VD Process
Controlling of Deleterious Elements in Bearing Steel GCrl5 Produced by 150 t LD-LF + RH Flow Sheet
LF Refining Slag System Optimization and Industrial Testing for 65Mn Steel
Optimization of Power Supply Curves for a 120 t LF
Process Practice for Spring Steel 65 Mn Produced by 80 t Combined Blown Converter-LF-CC Flow Sheet

Related Author

谯明亮
尹雨群
耿建林
姚永宽
田伟
李晶
余健
徐明

Related Institution

南京钢铁集团股份有限公司
本钢集团公诃炼钢厂
Ningbo Iron and Steel Co., Ltd.
邯郸钢铁集团公司
重庆钢铁股份有限公司
0