Thermodynamic Calculation and Experimental Analysis on Equilibrium Phases in Nickel Base Alloy Inconel 690
更新时间:2026-01-21
    • Thermodynamic Calculation and Experimental Analysis on Equilibrium Phases in Nickel Base Alloy Inconel 690

    • Special Steel   Vol. 29, Issue 4, Pages: 13-15(2008)
    • Received:22 January 2008,

      Online First:23 December 2022,

      Published:23 December 2008

    移动端阅览

  • 丰涵, 宋志刚, 郑文杰, et al. Thermodynamic Calculation and Experimental Analysis on Equilibrium Phases in Nickel Base Alloy Inconel 690[J]. Special Steel, 2008, 29(4): 13-15. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Heat Treatment Process on Mechanical Properties of High Chromium Low Activated Ferritic-martensitic Steel
Thermodynamic Calculation and Analysis on Equilibrium Phases Transformation in SA508-3 Steel
Thermodynamic Calculation and Analysis on Precipitated Phases in Heat-Resistant Steel T91
Effect of Titanium Content on Mechanical Properties of Nickel Base Alloy Inconel 690
Thermodynamic Calculation on Equilibrium Precipitated Phases in Martensitic Stainless Steel 9Cr18Mo

Related Author

Zhou Zhu
Xu Amin
Wang Shaobing
Su Cheng
Shen Qiang
Sun Wenqiang
陈红宇
刘正东

Related Institution

Zhejiang Jiuli Metal Materials Research Institute Co., Ltd.
Zhejiang Jiuli Hi-Tech Metals Co., Ltd.
Huzhou University
昆明理工大学材料与冶金工程学院
北京科技大学冶金与生态工程学院
0