Affecting Factors Analysis and Numerical Simulation for Hot Charging of Cast Bloom of Heavy Rail Steel
|更新时间:2026-01-21
|
Affecting Factors Analysis and Numerical Simulation for Hot Charging of Cast Bloom of Heavy Rail Steel
Special SteelVol. 29, Issue 5, Pages: 52-53(2008)
作者机构:
包头钢铁集团公司,1技术中心,2炼钢厂,包头,014010
作者简介:
基金信息:
DOI:
CLC:
Received:14 March 2008,
Online First:09 January 2023,
Published:09 January 2008
稿件说明:
移动端阅览
李峰, 史凤武, 董珍, et al. Affecting Factors Analysis and Numerical Simulation for Hot Charging of Cast Bloom of Heavy Rail Steel[J]. Special Steel, 2008, 29(5): 52-53.
DOI:
李峰, 史凤武, 董珍, et al. Affecting Factors Analysis and Numerical Simulation for Hot Charging of Cast Bloom of Heavy Rail Steel[J]. Special Steel, 2008, 29(5): 52-53.DOI:
Affecting Factors Analysis and Numerical Simulation for Hot Charging of Cast Bloom of Heavy Rail Steel
The models for temperature of hot delivery and charging of 280 mm x 380 mm cast bloom and liquid steel cooling from mold to secondary cooling area and air cooling area have been established and the effect of oxygen and nitrogen content in heavy rail steels U71Mn( % :0.66-0.76C
0.15-0.35Si
1.10-1.40Mn) and U75V (% : 0.70-0.78C
0.50-0.70Si
0.75-1.05Mn
0.04-0.08V)
cast bloom microstructure and bloom transport roller at inlet of reheating furnace on hot charging of bloom was analyzed by definite difference method. Simulation results show that the reheating time for cast bloom of heavy rail steel is saved by 40 min
and the service temperature of bloom transport roller is 250 ℃.