Effect of Tempering Temperature on Structure and Mechanical Properties of Steel 15CrMoV Direct-Water-Quenched after Finishing Rolling
更新时间:2026-01-21
    • Effect of Tempering Temperature on Structure and Mechanical Properties of Steel 15CrMoV Direct-Water-Quenched after Finishing Rolling

    • Special Steel   Vol. 30, Issue 2, Pages: 66-67(2009)
    • Received:29 September 2008,

      Online First:05 December 2022,

      Published:05 December 2009

    移动端阅览

  • 关婧, 蔡庆伍, 武会宾, et al. Effect of Tempering Temperature on Structure and Mechanical Properties of Steel 15CrMoV Direct-Water-Quenched after Finishing Rolling[J]. Special Steel, 2009, 30(2): 66-67. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effects of Quenching and Tempering Process on Yield to Tensile Strength Ratio of S770QL High Strength Seamless Tube
Research and Development of 10B21 Wire Rod for 8.8 Grade Non-quenched and Tempered Fasteners
Microstructure and Properties of 12Cr1MoVG Thick-wall Steel Pipe with High Temperature Normalizing + Tempering
Precipitation Behavior in Tempering of Cr-W-Mo-V Semi- High Speed Steel Containing Nitrogen
Effect of Tempering on Size and Orientation of Grain in Ultra-Fine Grain Bainite Steel

Related Author

Pan Xianming
Ma Jinhui
Fei Xingang
Li Fuhua
Du Kun
Zhang Jianfeng
Bai Yun
Kong Xiangwei

Related Institution

Daye Special Steel Co., Ltd.
Hubei Provincial Key Laboratory of High-quality Special Steel
Special Steel Institute, Jiangyin Xingcheng Special Steel works Co.,Ltd., Jiangyin
Steel Pipe Products Institute , Daye Special steel Co., Ltd.
Hubei province Key Laboratory for High Quality Special Steel
0