Influence of Nozzles Blocking of RH Up-Snorkel on Circulation Flow Rate
更新时间:2026-01-21
    • Influence of Nozzles Blocking of RH Up-Snorkel on Circulation Flow Rate

    • Special Steel   Vol. 30, Issue 5, Pages: 19-21(2009)
    • Received:09 April 2009,

      Online First:21 November 2022,

      Published:21 November 2009

    移动端阅览

  • 艾新港, 包燕平, 岳峰, et al. Influence of Nozzles Blocking of RH Up-Snorkel on Circulation Flow Rate[J]. Special Steel, 2009, 30(5): 19-21. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

A Study of Water Modeling on Circulation Flow Rate in RH Vacuum Refining Process
Industrial Experimental Study on Removal of Inclusions in Steel by Nitrogen Addition and Release Method
A Study on Water Modeling for Steel Fluid Flow in a CSP Mold
A Study on Water Modeling of Ladle with Bottom Argon Blowing in Critical Slag Entrapment Condition
A Study on Bubble Behavior during Vacuum Treatment of Refining Furnace with Single Snorkel and Metallurgical Effect

Related Author

欧洪林
包燕平
岳峰
林路
Liu Jianhua
Zhang Yudi
He Yang
Li Wei

Related Institution

北京科技大学冶金工程研究院
Dongbei Special Steel Group Trade Co., Ltd.
Institute of Engineering Technology University of Science and Technology Beijing
广州珠江钢铁有限公司
特殊钢厂
0