A Study on Water Modeling of Fluid Flow in a Tundish for Horizontal Continuous Casting
|更新时间:2026-01-21
|
A Study on Water Modeling of Fluid Flow in a Tundish for Horizontal Continuous Casting
Special SteelVol. 30, Issue 4, Pages: 22-23(2009)
作者机构:
1. 北京科技大学冶金与生态工程学院,北京,100083
2. 衡阳钢管公司技术中心,衡阳,421001
作者简介:
基金信息:
DOI:
CLC:
Received:13 January 2009,
Online First:20 December 2022,
Published:20 December 2009
稿件说明:
移动端阅览
杨树峰, 李京社, 唐海燕, et al. A Study on Water Modeling of Fluid Flow in a Tundish for Horizontal Continuous Casting[J]. Special Steel, 2009, 30(4): 22-23.
DOI:
杨树峰, 李京社, 唐海燕, et al. A Study on Water Modeling of Fluid Flow in a Tundish for Horizontal Continuous Casting[J]. Special Steel, 2009, 30(4): 22-23.DOI:
A Study on Water Modeling of Fluid Flow in a Tundish for Horizontal Continuous Casting
According to actual 15 t tundish for casting 中120 mm pipe billet by horizontal continuous caster
the 1:1.5 water model system has been established to examine the flow field in local tundish and study the effect of flow control device on behavior of liquid flow in tundish. Results showed that the dead zone ratio in tundish obviously decreased by u- sing turbulence inhibitor
but it was limited to prolong the minimum residence time; the residence time of liquid steel in tundish obviously increased by using inlet launder and low dam to promote the inclusions floating.