Application of Strengthening Melting Technology for an 120 t Converter
更新时间:2026-01-21
    • Application of Strengthening Melting Technology for an 120 t Converter

    • Special Steel   Vol. 30, Issue 5, Pages: 47-49(2009)
    • Received:02 April 2009,

      Online First:18 November 2022,

      Published:18 November 2009

    移动端阅览

  • 陈爱梅, 李炯伟, 乔林琐, et al. Application of Strengthening Melting Technology for an 120 t Converter[J]. Special Steel, 2009, 30(5): 47-49. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Ractice of EF3 Ultra-low Phosphorus Smelting Process for High-grade Pipeline Welding Wire
Calculation Model of Converter Lime Addition Based on Multiple Linear Regression
The Smelting Process Improvement of 120 t Top-Bottom Combined Blown Converter with High-Carbon Turndown and Low Phosphorus Tapping
Process Practice of Hot Forging Microalloying Steel F40MnV by Converter
A Study on Simulation of Stirring and Scouring Action in Top and Bottom Combined Blown Converter at Chongqing Steel

Related Author

Hou Jianwei
Tang Qing
Cui Guibo
Su Yongze
Zhang Xingli
Qi Fengyou
Chen Jun
Su Chunyang

Related Institution

Qingdao Branch, CITIC Pacific Steel Research Institute
Institute of Technology, Daye Special Steel Co., Ltd.
Jingjiang Special Steel Co., Ltd., Jingjiang
No.1Steelmaking Plant , HBIS GROUP HANSTEEL COMPANY
Handan Vocational College of Science and Technology
0