Finite Element Simulation of Temperature Field of Titanium Alloy Rod during Rolling Process with Flat Triangle Pass
|更新时间:2026-01-21
|
Finite Element Simulation of Temperature Field of Titanium Alloy Rod during Rolling Process with Flat Triangle Pass
Special SteelVol. 30, Issue 4, Pages: 42-44(2009)
作者机构:
太原科技大学材料科学与工程学院,太原,030024
作者简介:
基金信息:
DOI:
CLC:
Received:02 February 2009,
Online First:20 December 2022,
Published:20 December 2009
稿件说明:
移动端阅览
帅美荣, 秦建平. Finite Element Simulation of Temperature Field of Titanium Alloy Rod during Rolling Process with Flat Triangle Pass[J]. Special Steel, 2009, 30(4): 42-44.
DOI:
帅美荣, 秦建平. Finite Element Simulation of Temperature Field of Titanium Alloy Rod during Rolling Process with Flat Triangle Pass[J]. Special Steel, 2009, 30(4): 42-44.DOI:
Finite Element Simulation of Temperature Field of Titanium Alloy Rod during Rolling Process with Flat Triangle Pass
MSC.Marc finite element simulation software and contact analysis technique were used to simulate the three-dimensional heat deformation of TC4 ,titanium alloy (%:0.08C
6Al
4V
0.3Fe
0.05N
0.015H
balance Ti) Φ32 mm rod during rolling process with flat triangle pass and quantitatively to analyze the temperature field of rolling stock. Results showed that with beginning rolling temperature 950 ℃
the deformation of TC4 rod in flat triangle pass was stale and uniform
but there existed a temperature gradient along cross section of rod with lowest temperature 910 ℃ and highest temperature 966 ℃.