Effect of Ti-Nb on Formability of Annealed Cold Rolled Sheet of Ultra-Low Carbon Ferrite Stainless Steel Cr18
更新时间:2026-01-21
    • Effect of Ti-Nb on Formability of Annealed Cold Rolled Sheet of Ultra-Low Carbon Ferrite Stainless Steel Cr18

    • Special Steel   Vol. 30, Issue 6, Pages: 49-51(2009)
    • Received:13 May 2009,

      Online First:29 November 2022,

      Published:29 November 2009

    移动端阅览

  • 孙丹, 陈伟庆, 何慎, et al. Effect of Ti-Nb on Formability of Annealed Cold Rolled Sheet of Ultra-Low Carbon Ferrite Stainless Steel Cr18[J]. Special Steel, 2009, 30(6): 49-51. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Impact of the Annealing Temperature on the Magnetic and Mechanical Characteristics of Thin-gauge Non-oriented Electrical Steel
Effect of Aging Rolling Temperature on the Microstructure, Texture and Magnetic Properties of Low-temperature Grain-oriented Silicon Steel
Effect of Rolling Process on Texture Evolution of Cold Rolled Non-Oriented Silicon Steel
Effect of Yttrium Content on Microstructure and Texture of 3 % Si Oriented Silicon Steel
Evolution of Asynchronous Cold Rolling Texture in Thickness Direction of Non-Oriented Silicon Electric Steel

Related Author

Guo Han
Li Yadong
Dong Linshuo
Sun Chao
Li Fuqiang
Geng Zhiyu
Liu Xuming
Yin Licheng

Related Institution

Silicon Steel Division, Anshan Steel Co., Ltd.
Ansteel Beijing Research Institute Co., Ltd.
The State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology
Hongwang Holding Group, Hunan Hongwang New Material Technology
College of Material Science and Engineering, Shenzhen University
0