Influence of Solution Temperature on Structure and Corrosion Resistance of Plate of Super Duplex Stainless Steel S32750
更新时间:2026-01-21
    • Influence of Solution Temperature on Structure and Corrosion Resistance of Plate of Super Duplex Stainless Steel S32750

    • Special Steel   Vol. 30, Issue 2, Pages: 61-62(2009)
    • Received:25 September 2008,

      Online First:05 December 2022,

      Published:05 December 2009

    移动端阅览

  • 李国平, 李俊, 张威, et al. Influence of Solution Temperature on Structure and Corrosion Resistance of Plate of Super Duplex Stainless Steel S32750[J]. Special Steel, 2009, 30(2): 61-62. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effects of Solution Temperature on Microstructure and Tensile Properties of a Novel Ni-Co-Based Wrought Superalloy
Effect of Annealing Temperature on Structure of 0.2C-1.5Si-1.5Mn-(0.5Cu)TRIP Steel
Structure and Properties of Coarse Grain Heat Affected Zone of Zr Microalloying HSLA Steel
Structure and Properties of Low Carbon Sheet produced by FTSR Concasting Thin Slab Continuous Rolling Process at Tangshan Iron and Steel
Effect of Deformation on Structure and Mechanical Properties of Non-Orientation Silicon Steel 50W470

Related Author

Tian Peiyu
Wang Mingshi
Li Xinyu
景财年
王作成
李长龙
罗辉
李成美

Related Institution

Baowu Special Metallurgy Co., Ltd.
Gaona Aero Material Co.,Ltd.
山东建筑工程学院材料系
山东大学材料科学与工程学院
武汉钢铁(集团)公司技术中心
0