Effect of Dynamic Soft Reduction in Casting on Porosity and Inclusions in Heavy Rail of Steel U75V
|更新时间:2026-01-21
|
Effect of Dynamic Soft Reduction in Casting on Porosity and Inclusions in Heavy Rail of Steel U75V
Special SteelVol. 30, Issue 4, Pages: 57-58(2009)
作者机构:
1. 包头钢铁集团公司技术中心,包头,014010
2. 北京科技大学冶金学院,北京,100083
作者简介:
基金信息:
DOI:
CLC:
Received:11 February 2009,
Online First:20 December 2022,
Published:20 December 2009
稿件说明:
移动端阅览
李峰, 刘平, 董珍, et al. Effect of Dynamic Soft Reduction in Casting on Porosity and Inclusions in Heavy Rail of Steel U75V[J]. Special Steel, 2009, 30(4): 57-58.
DOI:
李峰, 刘平, 董珍, et al. Effect of Dynamic Soft Reduction in Casting on Porosity and Inclusions in Heavy Rail of Steel U75V[J]. Special Steel, 2009, 30(4): 57-58.DOI:
Effect of Dynamic Soft Reduction in Casting on Porosity and Inclusions in Heavy Rail of Steel U75V
6 Soft reduction stands are installed at each strand of 6 strands caster for 280 mm×380 mm bloom. The soft reduction in height of bloom is ≤8 mm wih reduction rate≤1.5mm/m.Results showed that with suitable process conditions and using dynamic soft reduction technology
the center porosity of bloom was improved led to obviously improve the center stripe at waist of heavy rail of steel U75V
and the rejection rate by non-destructive testing decreased from 0.206% to0.095% due to improvement of distribution of inclusions in bloom.