Study on Ultra-Low Carbon Bainite Steel DB800
更新时间:2026-01-21
    • Study on Ultra-Low Carbon Bainite Steel DB800

    • Special Steel   Vol. 30, Issue 5, Pages: 58-59(2009)
    • Received:23 April 2009,

      Online First:18 November 2022,

      Published:18 November 2009

    移动端阅览

  • 陈忠伟, 江雅民. Study on Ultra-Low Carbon Bainite Steel DB800[J]. Special Steel, 2009, 30(5): 58-59. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Precipitate Phase Pretreatment on Microstructure and Mechanical Properties of High-strength Bolts
Effect of C and Mo Content on Microstructure and Short-term Properties of IN617 Heat-resistant Alloy
Effect of Tempering Temperature on Microstructure and Mechanical Properties of High Co-Ni Secondary Hardening Steel
Effect of Cold-rolled Deformation on the Microstructure and Properties of GH4169 Alloy for Nuclear Power
Effect of Heat Treatment Process on Microstructure and Properties of Forged 430F Ferritic Stainless Steel

Related Author

Wang Xu
Wang Ying
Wang Yang
Zhou Lei
Tang Zhengxin
Li Gen
Li Ling
He Guanze

Related Institution

Special Steel Division, Nanjing Iron & Steel Co., Ltd.
Institute for Special Steels, Central Iron and Steel Research Institute Co., Ltd. (CISRI)
Shanghai Nuclear Engineering Research & Design Institute Co
Collaborative Innovation Center of Steel Technology, University of Science and Technology Beijing
Technology Center, Fushun Special steel Co., Ltd.
0