Effect of Austenizing Time on Structure and Properties of DP780 Cold Rolled Dual Phase Steel
更新时间:2026-01-21
    • Effect of Austenizing Time on Structure and Properties of DP780 Cold Rolled Dual Phase Steel

    • Special Steel   Vol. 31, Issue 5, Pages: 58-60(2010)
    • Received:25 March 2010,

      Online First:12 November 2022,

      Published:12 November 2010

    移动端阅览

  • 潘恩宝, 邸洪双, 蒋光炜, et al. Effect of Austenizing Time on Structure and Properties of DP780 Cold Rolled Dual Phase Steel[J]. Special Steel, 2010, 31(5): 58-60. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Production Process Practice of 42CrMoM Steel for 12.9 Grade High Strength Wind Power Fasteners
Effect of Mo Microalloying on High Temperature Mechanical Properties and Microstructure of 82B Steel
Controlled Rolling and Cooling Process Optimization of Non-annealed 12Cr1MoV Wire Rod Products for Boiler Flat Steel
Current Status and Prospects of Fatigue Performance for 300M Steel by Single Vacuum Process for Landing Gear of Commercial Aircraft
High Temperature Properties of Slab of Stainless Steels and Application in Concasting Secondary Cooling Process

Related Author

Liu Yueyun
Wang Zhanzhong
Zhang Yue
Li Xu
Liu Dan
Guo Shibei
Peng Feng
Wang Weimin

Related Institution

Research Institute, Daye Special Steel Co., Ltd.
Hubei Provincial Key Laboratory of High-quality Special Steel
School of Materials Science and Engineering, Guilin University of Technology
Key Laboratory of Nonferrous Metals and Materials Processing New Technology, Ministry of Education,Guilin University of Technology
Chongqing Polycomp International Corporation
0