您当前的位置:
首页 >
文章列表页 >
A Study on Bubble Behavior during Vacuum Treatment of Refining Furnace with Single Snorkel and Metallurgical Effect
更新时间:2026-01-21
    • A Study on Bubble Behavior during Vacuum Treatment of Refining Furnace with Single Snorkel and Metallurgical Effect

    • Special Steel   Vol. 31, Issue 5, Pages: 18-21(2010)
    • Received:13 May 2010,

      Online First:11 November 2022,

      Published:11 November 2010

    移动端阅览

  • 秦哲, 朱梅婷, 成国光, et al. A Study on Bubble Behavior during Vacuum Treatment of Refining Furnace with Single Snorkel and Metallurgical Effect[J]. Special Steel, 2010, 31(5): 18-21. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

A Study on Water Modeling for Steel Fluid Flow in a CSP Mold
Metallurgical Effect of Converter Smelting with Deep-Desulphurizing Hot Metal at Masteel
A Study on Water Modeling of Ladle with Bottom Argon Blowing in Critical Slag Entrapment Condition
Influence of Nozzles Blocking of RH Up-Snorkel on Circulation Flow Rate
A Study of Water Modeling on Circulation Flow Rate in RH Vacuum Refining Process

Related Author

景财良
王现辉
洪兵雄
柴毅忠
王新华
张炯明
吴明
吴发达

Related Institution

广州珠江钢铁有限公司
马钢股份有限公司第一钢轧总厂
北京科技大学冶金工程研究院
特殊钢厂
莱芜钢铁集团1技术中心,
0