Effect of Cooling Rate of Hot-Deformed Austenite on Structure and Property of X80 Pipeline Steel
更新时间:2026-01-21
    • Effect of Cooling Rate of Hot-Deformed Austenite on Structure and Property of X80 Pipeline Steel

    • Special Steel   Vol. 31, Issue 1, Pages: 63-65(2010)
    • Received:11 August 2009,

      Online First:27 October 2022,

      Published:27 October 2010

    移动端阅览

  • 曾宪平, 卢俊毅, 王文录. Effect of Cooling Rate of Hot-Deformed Austenite on Structure and Property of X80 Pipeline Steel[J]. Special Steel, 2010, 31(1): 63-65. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Holding Technology at Intermediate Roll Table in Hot Continuous Rolling on Phase Transformation and Structure of Low Carbon Steel
Effect of Cr on Phase Transformation and Structure of 0.035C-0.12Nb X80 Pipeline Steel
Development of Heavy Plate of Pre-hardened Plastic Die Steel 718
Effect of Rolling Process on Structure, Texture and Properties of X80 Pipeline Steel
Effect of Cooling Rate on Structure of Hot Rolled Round Bar of Steel 40CrMo

Related Author

徐远军
赵刚
温盾
魏钢城
牛延龙
孙新军
刘清友
孙力军

Related Institution

武汉科技大学材料与冶金学院
武汉钢铁公司
昆明理工大学材料与冶金工程学院
钢铁研究总院结构材料研究所
湖南工业大学冶金工程学院
0