Finite Element Simulation for Medium-Heavy Plate of Low Carbon Steel Rolling with MAS Method
|更新时间:2026-01-21
|
Finite Element Simulation for Medium-Heavy Plate of Low Carbon Steel Rolling with MAS Method
Special SteelVol. 32, Issue 1, Pages: 9-12(2011)
作者机构:
武汉科技大学材料与冶金学院,武汉,430081
作者简介:
基金信息:
DOI:
CLC:
Online First:26 September 2022,
Published:26 September 2011
稿件说明:
移动端阅览
张春林, 程晓茹, 董述峰, et al. Finite Element Simulation for Medium-Heavy Plate of Low Carbon Steel Rolling with MAS Method[J]. Special Steel, 2011, 32(1): 9-12.
DOI:
张春林, 程晓茹, 董述峰, et al. Finite Element Simulation for Medium-Heavy Plate of Low Carbon Steel Rolling with MAS Method[J]. Special Steel, 2011, 32(1): 9-12.DOI:
Finite Element Simulation for Medium-Heavy Plate of Low Carbon Steel Rolling with MAS Method
Based on works rolling process of 4300 mm medium-heavy plate of low carbon steel Q235 (C ≤0. 20% ) the elastic-plastic finite element model is established by using the finite element software ABAQUS/Explicit to simulate and calculate the general rolling process and MAS (Mizushima automatic plan view pattern control system) rolling process for medium-heavy plate with spread ratio 1. 70 and finishing rolling elongation 7. 87
and the comparative analysis on different deformation stages is carried out. Results show that the plane shape of rolled medium-heavy plate is obviously improved by using MAS rolling method
its changed value in shape is directly related to the setting parameters at MAS rolling stage
and the MAS rolling optimum parameter i. e. △L×△h= 300 x3 is obtained by comparing the rolling results using different MAS parameters.