Development of Drawing Forming Process for Outside-Square Inside-Circular Tube based on Finite Element Simulation
更新时间:2026-01-21
    • Development of Drawing Forming Process for Outside-Square Inside-Circular Tube based on Finite Element Simulation

    • Special Steel   Vol. 32, Issue 3, Pages: 44-47(2011)
    • Received:25 December 2010,

      Online First:18 October 2022,

      Published:18 October 2011

    移动端阅览

  • 刘升, 王伯文, 林希峰. Development of Drawing Forming Process for Outside-Square Inside-Circular Tube based on Finite Element Simulation[J]. Special Steel, 2011, 32(3): 44-47. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Key Metallurgical Technologies for Smelting 1Cr13 Stainless Steel via ANS-OB Process
Metallurgical Equipment and Process Route for Stainless Steel Steelmaking
Selection and Application of Cold Rolling Mill for Stainless Steel
An Analysis on Coupled Thermal- Mechanical Simulation of Metal Deformation in Continuous Rolling of Compact Strip Production
Effect of Heat Treatment on Structure and Properties of A New Precipitation Hardening Stainless Steel 1Cr16Ni3Cu1MoW

Related Author

Lu Zhihao
Teng Xingze
Xu Mengchun
Jin Zhe
Fu Xianbin
Li Boyang
郝祥寿
王一德

Related Institution

State Key Laboratory of Metallic Materials for Marine Equipment and Applications
Iron & Steel Research Institute of Ansteel Group
中冶华天工程技术有限公司
太原钢铁(集团)有限公司
昆明理工大学材料冶金工程学院
0