Development of Secondary Cooling Water Distribution Model for Large-Size Round Bloom Casting
|更新时间:2026-01-21
|
Development of Secondary Cooling Water Distribution Model for Large-Size Round Bloom Casting
Special SteelVol. 32, Issue 3, Pages: 1-4(2011)
作者机构:
北京科技大学冶金与生态工程学院,北京,100083
作者简介:
基金信息:
DOI:
CLC:
Received:22 November 2011,
Online First:17 October 2022,
Published:17 October 2011
稿件说明:
移动端阅览
曾智, 韩占光, 李景, et al. Development of Secondary Cooling Water Distribution Model for Large-Size Round Bloom Casting[J]. Special Steel, 2011, 32(3): 1-4.
DOI:
曾智, 韩占光, 李景, et al. Development of Secondary Cooling Water Distribution Model for Large-Size Round Bloom Casting[J]. Special Steel, 2011, 32(3): 1-4.DOI:
Development of Secondary Cooling Water Distribution Model for Large-Size Round Bloom Casting
Based on main technical parameters of a new built Φ600 mm圆坯连铸二次冷却数学模型600 mm round bloom caster in steel works
a math model for heat transfer and solidification of one-dimensional non-steady state casting bloom with cylindrical coordinates has been established
and the casting speed
superheating degree and intensity of cooling on temperature of casting bloom is analyzed by using finite differential method to solve and assemble program to carry out the calculation of temperature field of bloom with a given water flow rate. It is obtained with calculation on casting Φ500 mm bearing steel GCr15SiMn bloom that with every increasing casting speed 0. 1 m/min
the thickness of solidified shell of bloom at outlet of mold decreases by 7. 9 mm and the solidification terminal point is prolonged by 6. 7 m.