Finite Element Analysis of Effect Factors on Folding Defect of Medium and Heavy Plate
更新时间:2026-01-21
    • Finite Element Analysis of Effect Factors on Folding Defect of Medium and Heavy Plate

    • Special Steel   Vol. 32, Issue 2, Pages: 5-7(2011)
    • Online First:08 November 2022,

      Published:08 November 2011

    移动端阅览

  • 张春林, 程晓茹, 任勇, et al. Finite Element Analysis of Effect Factors on Folding Defect of Medium and Heavy Plate[J]. Special Steel, 2011, 32(2): 5-7. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Finite Element Simulation on Temperature Field of 0.45C Steel Medium and Heavy Plate during Straightening Process and Residual Stress Analysis
Effect on Fatigue Failure Behavior Induced by Inclusions in GCr15 Bearing Steel Under Different Metallurgical Processes
Numerical Simulation of Two-roller Rotary Rolling Piercing of a New Heat-resistant Alloy SP2215 Seamless Pipe
Finite Element Simulation,Optimization and Stress Analysis on Blooming and Rolling Heavy Rail
Analysis on Action and Reaction Force between Slab and Rollers at Segment of Dynamic Soft Reduction and Application in Casting

Related Author

詹三林
尹皓
李春光
刘炼
Luo Haiwen
Hu Bin
Yin Qing
Shi Tao

Related Institution

Jiangying Xingcheng Special Steel Works Co., Ltd., Jiangying
Daye Special Steel Co., Ltd.
Changzhou Baoling Heavy & Industrial Machinery Co., Ltd.
School of Metallurgy and Ecological Engineering, University of Science and Technology Beijing
Jiangsu Wujin Stainless Steel Pipe Group Co., Ltd.
0