    • Study on Regularity of Temperature Reduction of IF Steel Slab Casting Liquid with 210 t Top and Bottom Combined Blown Converter-RH Flow Sheet

    • Special Steel   Vol. 32, Issue 1, Pages: 40-43(2011)
    • Received:17 September 2010,

      Online First:27 September 2022,

      Published:27 September 2011

    移动端阅览

  • 王毓男, 包燕平, 崔衡, et al. Study on Regularity of Temperature Reduction of IF Steel Slab Casting Liquid with 210 t Top and Bottom Combined Blown Converter-RH Flow Sheet[J]. Special Steel, 2011, 32(1): 40-43. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Hot Rolling Parameters on Deformation Resistance of Coarse-Grained Niobium Steel
Prediction of Molten Steel End Point Temperature in LF Based on Modified Artificial Neural Network
Development of Secondary Cooling Water Distribution Model for Large-Size Round Bloom Casting
Experimental Study on Hot Deformation Behavior and Math Models for Deformation Resistance of EA4T Axle Steel for High Speed Rail
A Deformation Resistance Model for Casting Slab of 0. 47C-0. 36Si-0. 67Mm Medium Carbon Steel in Low Temperature Rolling Process

Related Author

刘清友
孙新军
文建华
雷霆
阴树标
陶子玉
姜茂发
刘承军

Related Institution

钢铁研究总院结构材料研究所
昆明理工大学材料与冶金工程学院
东北大学材料与冶金学院
北京科技大学冶金与生态工程学院
北京科技大学冶金与生态学院.
0