Mechanical Properties and Corrosion Resistance of As-Cast Medium Nitrogen Austenite Stainless Steel for Glass Curtain Wall Connector
更新时间:2026-01-21
    • Mechanical Properties and Corrosion Resistance of As-Cast Medium Nitrogen Austenite Stainless Steel for Glass Curtain Wall Connector

    • Special Steel   Vol. 32, Issue 4, Pages: 53-56(2011)
    • Received:13 January 2011,

      Online First:03 November 2022,

      Published:03 November 2011

    移动端阅览

  • 王喜, 李忠华, 蒋庆林, et al. Mechanical Properties and Corrosion Resistance of As-Cast Medium Nitrogen Austenite Stainless Steel for Glass Curtain Wall Connector[J]. Special Steel, 2011, 32(4): 53-56. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

No data

Related Author

No data

Related Institution

No data
0