A Study on Prediction Models for Alloying Charging and End Analysis during Ladle Furnace Refining
|更新时间:2026-01-21
|
A Study on Prediction Models for Alloying Charging and End Analysis during Ladle Furnace Refining
Special SteelVol. 32, Issue 2, Pages: 8-10(2011)
作者机构:
1. 北京科技大学冶金与生态工程学院,北京,100083
2. 新余钢铁有限责任公司,新余,338000
作者简介:
基金信息:
DOI:
CLC:
Received:19 November 2010,
Online First:08 November 2022,
Published:08 November 2011
稿件说明:
移动端阅览
罗仁辉, 橙朱荣, 杨凌志. A Study on Prediction Models for Alloying Charging and End Analysis during Ladle Furnace Refining[J]. Special Steel, 2011, 32(2): 8-10.
DOI:
罗仁辉, 橙朱荣, 杨凌志. A Study on Prediction Models for Alloying Charging and End Analysis during Ladle Furnace Refining[J]. Special Steel, 2011, 32(2): 8-10.DOI:
A Study on Prediction Models for Alloying Charging and End Analysis during Ladle Furnace Refining
Based on refining data of 110 t ladle refining furnace at Xinyu Steel Works
the prediction models for alloys adding amount and end analysis during refining of low carbon microalloying steels in ladle furnace have been established. 50 heats refining results show that the prediction results for adding amount of Xinyu Nol medium carbon chromium alloy and molybdenum iron alloy is basically accurate and the degree of accuracy for prediction value of end analysis of Cr and Mo in steel is more than 95%.