Progress of Hot Coil-Box Technology Application for Stainless Steel Hot Continuous Rolling Production
更新时间:2026-01-21
    • Progress of Hot Coil-Box Technology Application for Stainless Steel Hot Continuous Rolling Production

    • Special Steel   Vol. 32, Issue 4, Pages: 23-25(2011)
    • Received:19 January 2011,

      Online First:01 November 2022,

      Published:01 November 2011

    移动端阅览

  • 薛春江, 章昕. Progress of Hot Coil-Box Technology Application for Stainless Steel Hot Continuous Rolling Production[J]. Special Steel, 2011, 32(4): 23-25. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Treatment Technology of EAF Dust at Stainless Steel Works
Present  Status  and  Development  Trend  of  Stainless  Steel  in  China
Parameters Optimization of Laminar Flow Cooling Model for 2250 mm Wide-Strip Hot Continuous Rolling
Progress of Research on Performance of Passive Films of Stainless Steels
Effect of Initial Temperature of Stainless Steel Liquid for VOD on Refining Efficiency

Related Author

马国军
倪红卫
薛正良
贺东风
田乃媛
程鹏辉
周正军
张扬

Related Institution

武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
北京科技大学
武汉钢铁(集团)公司热轧厂
武汉科技大学材料与冶金学院
华南理工大学材料科学与工程学院
0