Development of Energy Saving Cold Heading Steels by 100 t EAF-LF-CC-CR Flow Sheet
更新时间:2026-01-21
    • Development of Energy Saving Cold Heading Steels by 100 t EAF-LF-CC-CR Flow Sheet

    • Special Steel   Vol. 32, Issue 4, Pages: 18-22(2011)
    • Received:19 January 2011,

      Online First:01 November 2022,

      Published:01 November 2011

    移动端阅览

  • 麻晗, 峰公雄. Development of Energy Saving Cold Heading Steels by 100 t EAF-LF-CC-CR Flow Sheet[J]. Special Steel, 2011, 32(4): 18-22. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Development of Undersea Linepipe Steel HSL450S
Development of Hot Rolled Strip of Niobium Microalloying Steel TL1114Nb for Rear Axle Crossbeam of Auto at Nanjing Steel
Development of Chromium-Free Passivating and Finger-Mark Proofing Hot-Dip Zinc-Coated Steel Sheet
Research and Development on ML45Mn2  Cold Heading Steel Wire Rod
Development of High Carbon Microalloying Non-Quenched-Tempered Steel C70S6 and Process Practice

Related Author

贺道中
肖鸿光
郜书忠
仇必宁
李军
孔凡庆
程晓杰
贾松

Related Institution

衡阳华菱钢管(集团)技术中心
湖南工业大学冶金校区
南京钢铁联合有限公司带钢厂
首钢冷轧薄板有限公司
湖南华菱湘潭钢铁有限公司技术质量部
0