Development and Application of Premelted Slag for Electroslag Remelting Process
更新时间:2026-01-21
    • Development and Application of Premelted Slag for Electroslag Remelting Process

    • Special Steel   Vol. 32, Issue 3, Pages: 17-19(2011)
    • Received:17 December 2010,

      Online First:17 October 2022,

      Published:17 October 2011

    移动端阅览

  • 姜周华, 董艳伍, 张新法, et al. Development and Application of Premelted Slag for Electroslag Remelting Process[J]. Special Steel, 2011, 32(3): 17-19. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Low-cost Non-vacuum Induction Furnace Smelting of High Molybdenum Content of Nickel-base Alloy
Quality Control of SWRH82B Steel Coil for Prestressed Wire at Xiangtan Steel
Development of Voltage Swing Control System of 15 t Consarc ESR Furnace
Quality Control of Bar Products of Bearing Steel Produced by Consteel EAF-LF(VD)-CC Process at Wuhan Iron and Steel
Influence of ESR Slag on Cleanness of GCr15 Bearing Steel

Related Author

Guo Jing
Wu Zhilong
Han Kui
Zhao Yue
Chen Xiuqiang
Wang Shucai
薛正良
王贵容

Related Institution

Technical Centre, Fushun Special Steel Co., Ltd.
湘潭钢铁集团公司
湖北省钢铁冶金重点实验室,武汉科技大学
清华大学自动化系
冶金自动化研究设计院
0