Effect of Austenizing Temperature on Structure and Mechanical Properties of Steel 30 Cr3 SiMnNiWMo
|更新时间:2026-01-21
|
Effect of Austenizing Temperature on Structure and Mechanical Properties of Steel 30 Cr3 SiMnNiWMo
Special SteelVol. 32, Issue 4, Pages: 60-63(2011)
作者机构:
1. 昆明理工大学冶金与能源工程学院,昆明,650093
2. 钢铁研究总院结构材料研究所,北京,100081
3. 河南省工业学校机电系,郑州,450053
作者简介:
基金信息:
DOI:
CLC:
Received:09 February 2011,
Online First:03 November 2022,
Published:03 November 2011
稿件说明:
移动端阅览
路妍, 王军华, 苏杰, et al. Effect of Austenizing Temperature on Structure and Mechanical Properties of Steel 30 Cr3 SiMnNiWMo[J]. Special Steel, 2011, 32(4): 60-63.
DOI:
路妍, 王军华, 苏杰, et al. Effect of Austenizing Temperature on Structure and Mechanical Properties of Steel 30 Cr3 SiMnNiWMo[J]. Special Steel, 2011, 32(4): 60-63.DOI:
Effect of Austenizing Temperature on Structure and Mechanical Properties of Steel 30 Cr3 SiMnNiWMo
The effect of austenitic treatment at 860 ~ 980 °C on microstructure of steel 30CrSiMnNiWMo (% :0. 28C
0. 74Mn
1. 04Si
2. 70Cr
1. 15Ni
0. 45Mo
1.04W
0. 07V
0. 05Al) and mechanical properties of steel tempered at 260 °C has been studied. Results show that there are a lot of carbide M6C in microstructure of steel 30Cr3SiMnNiWMo quenched at 860 ~ 920 °C led to slightly decrease toughness of tempered steel
and after quenched at 950 °C
the carbides in steel are basically dissolved and the original austenite grains of steel beginning coarsen led to de- crease strength of tempered steel ; with oil quenched at 920 ℃ for 1 h + tempered at 260 °C for 2 h
the steel 30Cr3SiMnNiWMo has lath martensite microstructure with minor residual austenite and un-dissolved carbides
so it has excellent strength and toughness i. e. UTS- 1 680 MPa