Mathematical Simulation for Optimization of Tundish with Gas Curtain and Its Metallurgy Effects
|更新时间:2026-01-21
|
Mathematical Simulation for Optimization of Tundish with Gas Curtain and Its Metallurgy Effects
Special SteelVol. 32, Issue 2, Pages: 37-40(2011)
作者机构:
1. 首钢水城钢铁(集团)有限责任公司,六盘水,553028
2. 北京联合荣大工程材料有限责任公司,北京,101400
3. 武汉科技大学省部共建耐火材料与高温陶瓷国家重点实验室培育基地,武汉,430081
作者简介:
基金信息:
DOI:
CLC:
Received:23 November 2010,
Online First:09 November 2022,
Published:09 November 2011
稿件说明:
移动端阅览
马光林, 皮怀玉, 龚荣波, et al. Mathematical Simulation for Optimization of Tundish with Gas Curtain and Its Metallurgy Effects[J]. Special Steel, 2011, 32(2): 37-40.
DOI:
马光林, 皮怀玉, 龚荣波, et al. Mathematical Simulation for Optimization of Tundish with Gas Curtain and Its Metallurgy Effects[J]. Special Steel, 2011, 32(2): 37-40.DOI:
Mathematical Simulation for Optimization of Tundish with Gas Curtain and Its Metallurgy Effects
According to structure and operation parameters of a 32 t tundish for 150 mm X 150 mm 6-strand concasting billet at steelmaking workshop
Shuicheng Steel
the effect of gas curtain technology on characteristics of liquid flow in tundish and removal rate of inclusion particles in steel has been studied by using mathematical simulation method
and the commercial test for casting HPB235 and 65 C steel is carried out. Results show that the gas curtain weir is available to improve flow situation of liquid
balance residence time at each outlet
effectively prolong the residence time of liquid in tundish
decrease dead zone volume and increase removal rate of inclusion particles. This technology is suitable to meet the requirement for cleanliness steel steelmaking with tundish for multi-strand casting.