胡支国, 潘江, 陈敏, et al. Practice of Process for Steel 80Mnl4 Produced by 30 t EBT Arc Furnace-LF-CC Flow Sheet[J]. Special Steel, 2011, 32(4): 47-49.
DOI:
胡支国, 潘江, 陈敏, et al. Practice of Process for Steel 80Mnl4 Produced by 30 t EBT Arc Furnace-LF-CC Flow Sheet[J]. Special Steel, 2011, 32(4): 47-49. DOI:
通过采用电弧炉出钢前在钢包中加入40%的锰铁
LF精炼前期调整成分
精炼中期和末期控制精炼渣碱度≥2.5
软吹氩搅拌
控制中间包钢水过热度≤35℃
连铸全程进行保护浇铸等工艺措施
贵阳特钢—炼钢厂成功进行了80Mn14钢(%:0.75~0.96C、13.00~15.50Mn、≤0.80Si、≤0.070P、≤0.030S)的30 t EBT AF-35 t LF-260mm×300mm连铸机流程生产
产品各项性能均满足标准要求。
With using the process measures including adding 40% of needed ferromanganese amount in ladle before tapping of arc furnace
adjusting analysis of liquid in earlier stage of LF refining
controlling refining slag basicity N2. 5 and soft argon stirring in middle and last stage of refining
controlling overheating of liquid in tundish ≤35 ℃ and whole process shielding casting
the steel 80Mnl4 (%:0.75〜0.96C
13. 00 - 15. 50Mn
≤ 0.80Si
≤0.070P
≤ 0.030S) is successfully produced by 30 t EBT AF-35 t LF-260 mm x 300 mm caster flow sheet at Nol Steelmaking Works
Guiyang Steel
and all properties of products meet the requirement of standard.