Numerical and Physical Simulation on Fluid Flow Field in Mold of Vertical Slab Caster
更新时间:2026-01-21
    • Numerical and Physical Simulation on Fluid Flow Field in Mold of Vertical Slab Caster

    • Special Steel   Vol. 33, Issue 1, Pages: 15-17(2012)
    • Received:18 September 2011,

      Online First:19 September 2022,

      Published:19 September 2012

    移动端阅览

  • 赵志刚, 盘施哲, 胡坤太, et al. Numerical and Physical Simulation on Fluid Flow Field in Mold of Vertical Slab Caster[J]. Special Steel, 2012, 33(1): 15-17. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

A Study on Water Model for Liquid Level Fluctuation and Impact Depth of Flow in Mold for Slab Casting
A Study on Distribution Characteristics of Electromagnetic Field in Concasting Mould for Round Bloom
Analysis on Clogging of Submerged Entry Nozzle for 409L Stainless Steel Concasting and Improved Measure
Model for Changing of MnO Content in Mold Flux during Concasting
Study and Application on Physical Simulation of Single Thick Slab Flow Tundish

Related Author

刘文华
童志博
刘红军
王建军
汪开忠
施晓芳
李卫国
周俐

Related Institution

武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
华菱涟源钢铁公司
宝山钢铁股份有限公司不锈钢分公司
北京科技大学冶金与生态工程学院
钢铁研究总院国家连铸中心
0