A mathematical model for 14. 5 t tundish casting 160 mm x 160 mm billet at Shougang is established and the numerical calculation of flow and temperature of liquid in shape tundish for 4-strand is calculated by using fluid dynamic software Fluent to get the flow speed field
temperature field and residence time distribution curves of liquid in tundish. Calculation results show that the maximum temperature difference between each strand is 8 K
therefore the lower overheating extent liquid shall be avoided; besides the percentage of dead volume of No l strand is 20% little larger than that other strands ( 10% 〜12% )
the flow parameters of liquid in tundish meet the requirement for casting operation.
Research and Application Progress of Plasma Heating Technology for Continuous Casting Tundish
Calculation Model and Evolution Law of Temperature Field and Phase Precipitation along the Entire Line of Cold Heading Steel SCM435 High-Speed Wire Rod
Thermodynamic Coupling Analysis of Air Cooling for X70 Pipeline Steel Continuous Casting Slab Based on ABAQUS
Simulation of Columnar Crystal Growth in Forced Flow of VAR Based on Phase Field Method
Research Progress on Numerical Simulation of Temperature Field during Directional Solidification of Nickel-based Single Crystal Turbine Blades
Related Author
Li Jingshe
Wang Cun
Chen Yongfeng
Yang Shufeng
Liu Wei
Bai Yun
Huang Chengyong
Sun Ye
Related Institution
School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing