A Study on Finite Element Simulation for Leveling Process of Steel Plate by Straightener with Nine-Roll
|更新时间:2026-01-21
|
A Study on Finite Element Simulation for Leveling Process of Steel Plate by Straightener with Nine-Roll
Special SteelVol. 33, Issue 1, Pages: 9-11(2012)
作者机构:
1. 武汉科技大学材料与冶金学院,武汉,430081
2. 武汉钢铁集团公司热轧总厂,武汉,430083
作者简介:
基金信息:
DOI:
CLC:
Received:30 August 2011,
Online First:19 September 2022,
Published:19 September 2012
稿件说明:
移动端阅览
张焕军, 程晓茹, 任勇, et al. A Study on Finite Element Simulation for Leveling Process of Steel Plate by Straightener with Nine-Roll[J]. Special Steel, 2012, 33(1): 9-11.
DOI:
张焕军, 程晓茹, 任勇, et al. A Study on Finite Element Simulation for Leveling Process of Steel Plate by Straightener with Nine-Roll[J]. Special Steel, 2012, 33(1): 9-11.DOI:
A Study on Finite Element Simulation for Leveling Process of Steel Plate by Straightener with Nine-Roll
研究了22 mm Q345钢板(/%:≤0.20C、≤O.55Si、≤1.70Mn、O.02~O.15V、0.015~0.060Nb、0.02~O.20Ti)在9辊矫直机矫直时首辊与尾辊的位置对钢板平直度和表面残余应力的影响
得到钢板不平的位置集中在尾部。1~#辊和9~#辊在高度上的自由调节
可以保证钢板出矫直机时不会出现上弯或下弯。钢板的上表面残余应力比下表面低
延钢板长度方向
钢板表面残余应力呈现尾部高、头部低的状态。
Abstract
The effect of first roll and last roll position on plate flatness and surface residual stress of 22 mm Q345 steel plate (/% : ≤0. 20C
≤ 0. 55Si
≤1. 70Mn
0. 02 - 0. 15V
0. 015 ~ 0. 060Nb
0. 02 ~ 0. 20Ti) during leveling process by a 9-roll straightener has been studied by established finite element model to get the position of un-flatness is mainly at tail of plate. With free adjustment of height of Nol (first) roll and No9 (last) roll the plate is ensured no-bending up and down as the plate is out of straightener. The residual stress at upper surface of plate is lower that at bottom surface
and along the length direction of plate
the residual stress at head of plate is lower than that at end of plate.