Test and Study on Reheating Process of 280 mm x 380 mm Cast Bloom of Steel U75V for Heavy Rail
|更新时间:2026-01-21
|
Test and Study on Reheating Process of 280 mm x 380 mm Cast Bloom of Steel U75V for Heavy Rail
Special SteelVol. 32, Issue 6, Pages: 36-39(2011)
作者机构:
武汉科技大学材料与冶金学院,武汉,430081
作者简介:
基金信息:
DOI:
CLC:
Received:27 May 2011,
Online First:18 October 2022,
Published:18 October 2011
稿件说明:
移动端阅览
孙志亮, 杭乃勤, 李浩进. Test and Study on Reheating Process of 280 mm x 380 mm Cast Bloom of Steel U75V for Heavy Rail[J]. Special Steel, 2011, 32(6): 36-39.
DOI:
孙志亮, 杭乃勤, 李浩进. Test and Study on Reheating Process of 280 mm x 380 mm Cast Bloom of Steel U75V for Heavy Rail[J]. Special Steel, 2011, 32(6): 36-39.DOI:
Test and Study on Reheating Process of 280 mm x 380 mm Cast Bloom of Steel U75V for Heavy Rail
The 280 mm x 380 mm cast bloom temperature of steel U75V for heavy rail in walking beam reheating furnace has been traced and measured by using Thermophil STOR measure system (black box) at steel works
and the data are treated by Origin software to get the curves of cast bloom heating temperature
temperature increasing speed and difference of temperature between bloom surface and center etc. Results show that the average heating temperature of cast bloom is 1 220 °C
as heating time in furnace is more than 180 min
the control temperature in soaking zone should decrease by a- bout 20 °C; the effect of water-cooling beam in furnace on temperature of bloom bottom surface is obvious
therefore the control temperature of lower section in soaking zone is higher 20 °C than that of upper section ; at current heating condition
it meets the requirement of heavy rail production that temperature differential between center and surface of finished heating bloom along the thickness direction is less than 20 °C and the cast bloom temperature is more than 1 200 °C.