A Regression Analysis on Chemical Composition and Mechanical Properties of Stainless Steel 1Cr15Ni4Mo3N Round Products
|更新时间:2026-01-21
|
A Regression Analysis on Chemical Composition and Mechanical Properties of Stainless Steel 1Cr15Ni4Mo3N Round Products
Special SteelVol. 33, Issue 1, Pages: 63-64(2012)
作者机构:
1. 钢铁研究总院结构材料研究所,北京,100081
2. 抚顺特殊钢股份有限公司,抚顺,113001
作者简介:
基金信息:
DOI:
CLC:
Received:08 August 2011,
Online First:21 September 2022,
Published:21 September 2012
稿件说明:
移动端阅览
孙永庆, 梁剑雄, 杨志勇, et al. A Regression Analysis on Chemical Composition and Mechanical Properties of Stainless Steel 1Cr15Ni4Mo3N Round Products[J]. Special Steel, 2012, 33(1): 63-64.
DOI:
孙永庆, 梁剑雄, 杨志勇, et al. A Regression Analysis on Chemical Composition and Mechanical Properties of Stainless Steel 1Cr15Ni4Mo3N Round Products[J]. Special Steel, 2012, 33(1): 63-64.DOI:
A Regression Analysis on Chemical Composition and Mechanical Properties of Stainless Steel 1Cr15Ni4Mo3N Round Products
The analysis on elements content in 58 heats stainless steel 1Cr15Ni4Mo3N (/% : 0. 11 ~0. 16C
0. 50 〜 1. 25Mn
W0. 70Si
4. 0 ~5. 0Ni
14. 5 ~ 15. 5Cr
2. 3 ~2. 8Mo
0. 05 ~0. IN) random sampling from φ60 ~90 mm bars are carried out
while the longitudinal mechanical properties of each heat products heat-treated with 1 070 ℃ 1 h
air cooling
一70℃ 4 h cold treatment then 200℃ 2 h tempering are measured. The regression equations between the chemical composition and the mechanical properties of steel are obtained by statistic regression analysis.