Effect of Finishing Temperature and Cooling Rate on Structure and Mechanical Properties of Steel Q550D
|更新时间:2026-01-21
|
Effect of Finishing Temperature and Cooling Rate on Structure and Mechanical Properties of Steel Q550D
Special SteelVol. 33, Issue 3, Pages: 57-60(2012)
作者机构:
南京钢铁联合有限公司技术质量部,南京,210035
作者简介:
基金信息:
DOI:
CLC:
Received:07 November 2011,
Online First:14 October 2022,
Published:14 October 2012
稿件说明:
移动端阅览
高兵, 赵亚娟. Effect of Finishing Temperature and Cooling Rate on Structure and Mechanical Properties of Steel Q550D[J]. Special Steel, 2012, 33(3): 57-60.
DOI:
高兵, 赵亚娟. Effect of Finishing Temperature and Cooling Rate on Structure and Mechanical Properties of Steel Q550D[J]. Special Steel, 2012, 33(3): 57-60.DOI:
Effect of Finishing Temperature and Cooling Rate on Structure and Mechanical Properties of Steel Q550D
The effect of finishing temperature (800 ~850 °C ) and cooling rate (2 〜20 ℃/s) on structure and mechanical properties of microalloying steel Q55OD plate (/% : 0. 06C
0. 20Si
I. 60Mn
0. 010P
0. 001S
0. 10Mo
0. 06Nb
0. 01V
0. 02Ti) has been studied by using thermo-mechanical simulator Gleeble-3800. Results show that with decreasing finishing temperature and increasing cooling rate after rolling
the granular bainite in steel gradually decreases
and the lath bainite gradually increases
as a results the yield and tensile strength of steel increasing trend is obvious and the - 20 ℃ toughness is improved but the elongation of steel is decreasing trend ; with finishing temperature 850 °C and cooling rate 15 - 20 ℃/s the steel Q550D has better strength-toughness comprehensive properties