Physical and Mathematical Simulation of Structure Optimization of Dam in Tundish for Slab Continuous Casting
|更新时间:2026-01-21
|
Physical and Mathematical Simulation of Structure Optimization of Dam in Tundish for Slab Continuous Casting
Special SteelVol. 33, Issue 2, Pages: 14-17(2012)
作者机构:
1. 北京科技大学冶金工程研究院,北京,100083
2. 北京科技大学钢铁冶金新技术国家重点实验室,北京,100083
作者简介:
基金信息:
DOI:
CLC:
Received:12 October 2011,
Online First:13 October 2022,
Published:13 October 2012
稿件说明:
移动端阅览
苑品, 包燕平, 崔衡, et al. Physical and Mathematical Simulation of Structure Optimization of Dam in Tundish for Slab Continuous Casting[J]. Special Steel, 2012, 33(2): 14-17.
DOI:
苑品, 包燕平, 崔衡, et al. Physical and Mathematical Simulation of Structure Optimization of Dam in Tundish for Slab Continuous Casting[J]. Special Steel, 2012, 33(2): 14-17.DOI:
Physical and Mathematical Simulation of Structure Optimization of Dam in Tundish for Slab Continuous Casting
An analysis on fluid flowing status in a 60 t tundish with different dam structure for two-strand slab casting at Steel Works has been carried out by using geometric similarity ratio 0. 4 water model and Fluent math model. Results show that with using original structure- 200 mm height non-hole dam in tundish
the condition of liquid flow close to bottom of tundish is serious
and because of low dam
the effect of liquid lifting upward is not obvious
it is not available to remove inclusions from liquid and form large dead zone in casting area. As the height of dam increases to 270 mm with two upward 15° round hole
the minimum residence time of liquid in tundish increases by 12.5%
the dead zone decreases by 36%
the liquid flows toward surface of liquid in casting area
the dead zone in casting area and different temperature layer appearance basically disappear.