Water Modeling Test for Auxiliary Deslagging by Blowing Gas in Hot Metal Ladle
更新时间:2026-01-21
    • Water Modeling Test for Auxiliary Deslagging by Blowing Gas in Hot Metal Ladle

    • Special Steel   Vol. 33, Issue 3, Pages: 1-3(2012)
    • Received:01 November 2011,

      Online First:08 October 2022,

      Published:08 October 2012

    移动端阅览

  • 许飞, 沈巧珍, 栾国庆, et al. Water Modeling Test for Auxiliary Deslagging by Blowing Gas in Hot Metal Ladle[J]. Special Steel, 2012, 33(3): 1-3. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Water Modelling for a 85 t Top-Bottom Combined Blown Converter at Chongqing Steel
Measurement of Drag Coefficient in Slot Plug for Gas Stirring
Water Modelling Test on Interaction between Bottom Injection Gas and Bath for an 180 t Converter#br#
Physical and Mathematical Study on Flow Control Device of Tundish for 5-Strand billet Casting at Chongqing Steel
Experiment on Optimum Location of Bottom Nozzle in a 130 t Argon Stirred Ladle by Water Model

Related Author

鱼洋洋
唐萍
周亮
龙贻菊
陈文满
梁庆
安昌遐
周建安

Related Institution

重庆钢铁公司炼钢厂
重庆大学材料科学与工程学院
东北大学材料与冶金学院
中冶华天工程技术有限公司
辽宁科技大学材料学院,鞍山4
0