您当前的位置:
首页 >
文章列表页 >
Experimental Investigation on Effect of RH Refining Slag Series   and Desulfurization Agent on Desulfurization of Pipeline Steel
更新时间:2026-01-21
    • Experimental Investigation on Effect of RH Refining Slag Series   and Desulfurization Agent on Desulfurization of Pipeline Steel

    • Special Steel   Vol. 33, Issue 5, Pages: 12-14(2012)
    • Received:27 March 2012,

      Online First:09 October 2022,

      Published:09 October 2012

    移动端阅览

  • 姜桂连, 唐海燕, 程爱民, et al. Experimental Investigation on Effect of RH Refining Slag Series   and Desulfurization Agent on Desulfurization of Pipeline Steel[J]. Special Steel, 2012, 33(5): 12-14. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

A Study on Water Model for Circulation Flow Rate Optimization in RH Degassing Refining
Optimization and Production Practice of Top Slag Modifier for IF Steel DC06 with 260 t BOF-RH Flowsheet
A Test on Desulphurization of 12CaO•7Al2O3 Based Refining Slag
A Study on Desulphurization of Bearing Steel GCrl5 with LF Bearing BaO Refining Slag Series
Steelmaking Process and Quality Control of Cold-Heading Steel SWRCH35K by 120 t BOF-Argon Blowing-LF-CC Flowsheet

Related Author

包燕平
吴华杰
马鑫
贾楠
艾新港
胡巍
徐斌
黄嘉琦

Related Institution

河北钢铁集团邯钢分公司技术中心
河北钢铁集团邯钢分公司邯宝炼钢厂
武汉科技大学省部共建耐火材料与冶金国家重点实验室
南京钢铁股份有限公司中厚板卷厂
内蒙古科技大学材料与冶金学院
0