Present Status and Development Tendency of Patented Technology for High Strength Oil Well Tubing Steels
更新时间:2026-01-21
    • Present Status and Development Tendency of Patented Technology for High Strength Oil Well Tubing Steels

    • Special Steel   Vol. 33, Issue 5, Pages: 19-24(2012)
    • Received:30 March 2012,

      Online First:09 October 2022,

      Published:09 October 2012

    移动端阅览

  • 牟昊, 陈妍, 齐殿威, et al. Present Status and Development Tendency of Patented Technology for High Strength Oil Well Tubing Steels[J]. Special Steel, 2012, 33(5): 19-24. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Production Practice of Φ219.1mm x9.5mm Anti-Hydrogen Sulfide Corrosion Seamless Pipe Line Steel Tube X52QS
Effect of Normalizing Preheat Treatment on Structure and Properties of 42CrMo Forging Crankshaft Steel after Quenching and Tempering Treatment
Effect of Quenching and Tempering Treatment on Structure and Mechanical Properties of 22MnCrNiMo Steel Flash Weld Zone

Related Author

王学敏
邓叙燕
李健强
冯莹
李英真
胡楚江
李康丽
李永志

Related Institution

达力普石油专用管有限公司技术中心
河北省石油专用管工程技术研究中心
江西九江学院机械与材料工程学院
华中科技大学材料成形与模具技术国家重点实验室
江苏科技大学材料科学与工程学院
0