您当前的位置:
首页 >
文章列表页 >
Effect of C, Si Content in Liquid on Splashing during VOD Process Refining Stainless Steels
更新时间:2026-01-21
    • Effect of C, Si Content in Liquid on Splashing during VOD Process Refining Stainless Steels

    • Special Steel   Vol. 33, Issue 3, Pages: 26-28(2012)
    • Received:16 November 2011,

      Online First:13 October 2022,

      Published:13 October 2012

    移动端阅览

  • 安杰, 耿振伟, 李忠伟, et al. Effect of C, Si Content in Liquid on Splashing during VOD Process Refining Stainless Steels[J]. Special Steel, 2012, 33(3): 26-28. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Water Model Simulation Test for VOD Refining Process

Related Author

王东
包燕平
徐保美
李建民
李志斌
李道明

Related Institution

北京科技大学冶金与生态工程学院
太原钢铁(集团)有限公司
0