Metallurgy Effect of Argon Stirring after Oxygen Blow of an 120 t Top and Bottom Combined Blown Converter
|更新时间:2026-01-21
|
Metallurgy Effect of Argon Stirring after Oxygen Blow of an 120 t Top and Bottom Combined Blown Converter
Special SteelVol. 33, Issue 5, Pages: 38-39(2012)
作者机构:
1. 兰州资源环境职业技术学院,兰州,730021
2. 江西冶金职业技术学院,新余,338028
3. 河北科技大学材料科学与工程学院,石家庄,050018
作者简介:
基金信息:
DOI:
CLC:
Received:11 March 2012,
Online First:09 October 2022,
Published:09 October 2012
稿件说明:
移动端阅览
马琼, 胡秋芳, 冯捷. Metallurgy Effect of Argon Stirring after Oxygen Blow of an 120 t Top and Bottom Combined Blown Converter[J]. Special Steel, 2012, 33(5): 38-39.
DOI:
马琼, 胡秋芳, 冯捷. Metallurgy Effect of Argon Stirring after Oxygen Blow of an 120 t Top and Bottom Combined Blown Converter[J]. Special Steel, 2012, 33(5): 38-39.DOI:
Metallurgy Effect of Argon Stirring after Oxygen Blow of an 120 t Top and Bottom Combined Blown Converter
The converter post-blow argon stirring process may further promote carbon-oxygen reaction in liquid
effectively decreases converter end oxygen content in liquid. The results of commercial test of 120 t combined blown converter post-blow argon stirring process show that the post-blow argon stirring process may decreases the converter end carbon-oxygen product
with bottom blowing rate 800 m
3
/h argon stirring for 5 min
the [O]decreases to 400 x 10
-6
from 897 x 10
-6
before argon stirring; the (FeO) decreases to 13. 7% from 18. 5% ; the average [S] decreases to 0. 005% from 0. 009% and the average [P] decreases to 0. 006% from 0. 008%; after stirring for 3 ~6 min
the average temperature of liquid decreases 10 - 20 °C.