Application of Technology of Vibration-Excited Nucleation in Liquid during Ingot and Casting Slab Solidifying Process
更新时间:2026-01-21
    • Application of Technology of Vibration-Excited Nucleation in Liquid during Ingot and Casting Slab Solidifying Process

    • Special Steel   Vol. 33, Issue 6, Pages: 18-21(2012)
    • Received:28 May 2012,

      Online First:27 September 2022,

      Published:27 September 2012

    移动端阅览

  • 陶红标, 张慧, 王超, et al. Application of Technology of Vibration-Excited Nucleation in Liquid during Ingot and Casting Slab Solidifying Process[J]. Special Steel, 2012, 33(6): 18-21. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Control of Chemical Composition and Quality of LZ50 Steel Billet for Vehicle Axle Produced by 120 t Converter -LF + RH-TB Process
Application of Mold Electromagnetic Stirring Technology for 280 mm×380 mm Concasting Bloom
Effect of Electromagnetic Stirring on Temperature Field of ESR Ingot
Processing and Metallurgical Quality of Bearing Steel GCr15 Produced by 120 t Converter-LF-RH-CC Flow Sheet
Simulation Study and Application on Solidification Structure of E36 Steel Ship Slab

Related Author

王荣武
许家彦
陈永
朱苗勇
白海军
厉英
李宝宽
陈小龙

Related Institution

本溪钢铁集团公司
东北大学材料与冶金学院
攀枝花钢铁研究院材料研究所
攀枝花钢铁研究院
攀枝花新钢机股份有限公司
0