Numerical Simulation on Submerged Nozzle in Mold of Continuous Caster for Wider Slab
更新时间:2026-01-21
    • Numerical Simulation on Submerged Nozzle in Mold of Continuous Caster for Wider Slab

    • Special Steel   Vol. 34, Issue 1, Pages: 1-4(2013)
    • Received:11 July 2012,

      Online First:13 September 2022,

      Published:13 September 2013

    移动端阅览

  • 舒宏富, 刘浏, 刘学华. Numerical Simulation on Submerged Nozzle in Mold of Continuous Caster for Wider Slab[J]. Special Steel, 2013, 34(1): 1-4. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Influence of Immersion Depth of Long Nozzle on Flow Field and Temperature Field of Liquid Steel in a 36 t Tundish during Profiled Bloom Casting
Numerical Simulation of Effect of 420 mm x 1100 mm Slab Casting Mold Injecting Argon on Flow Field and Temperature Field of Liquid
Numerical Simulation of Flow Field in Mould for Slab Continuous Casting and Optimal Operation
Effect of Electromagnetic Stirring on Temperature Field of ESR Ingot
A Study on Water Model and Numerical Simulation of Flow Field in Slab Casting Mold with Different Width

Related Author

阮飞
赵凤光
富晓阳
刘卓承
杨吉春
张捷宇
孙健
贾凌锋

Related Institution

内蒙古科技大学材料与冶金学院
上海大学上海市现代冶金与材料制备重点实验室
江苏科技大学张家港校区冶金与材料工程学院,张家港
安徽工业大学冶金与资源学院
东北大学材料与冶金学院
0