Effect of Al, Ti, Nb Microalloying on Mixed Grain Size of Case-Hardened Steel ZF7
更新时间:2026-01-21
    • Effect of Al, Ti, Nb Microalloying on Mixed Grain Size of Case-Hardened Steel ZF7

    • Special Steel   Vol. 34, Issue 2, Pages: 52-54(2013)
    • Received:09 October 2012,

      Online First:08 October 2022,

      Published:08 October 2013

    移动端阅览

  • 李绍杰, 樊一丁, 黄胜永. Effect of Al, Ti, Nb Microalloying on Mixed Grain Size of Case-Hardened Steel ZF7[J]. Special Steel, 2013, 34(2): 52-54. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Nb-Ti on Structure and Properties of High Strength Weathering Steel
Effect of RE on Hot Plasticity of V Microalloying Heavy Rail Steel
Effect of Heat Treatment Process on Structure and Mechanical Properties of Steel Q345D for Rudder Stock
Effect of Ti-Nb Microalloying on Structure and Properties of Low Carbon High Strength Steel
Research Progress in Gear Steels for High Temperature Carburization

Related Author

康永林
谷海容
苏世怀
张建平
骆小刚
马玉平
陈庆军
安胜利

Related Institution

内蒙古科技大学
技术质量部
包头钢铁职业技术学院
包钢(集团)公司
技术中心
0