Analysis on Pen-Tip Shaped Fracture of SWRH82B Wire Rod and Process Improvement
更新时间:2026-01-21
    • Analysis on Pen-Tip Shaped Fracture of SWRH82B Wire Rod and Process Improvement

    • Special Steel   Vol. 34, Issue 4, Pages: 49-52(2013)
    • Received:01 March 2013,

      Online First:11 September 2022,

      Published:11 September 2013

    移动端阅览

  • 秦凤婷, 王红伟, 刘宗辉. Analysis on Pen-Tip Shaped Fracture of SWRH82B Wire Rod and Process Improvement[J]. Special Steel, 2013, 34(4): 49-52. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Concasting Technology Parameters on Center Carbon, Segregation of High Carbon Steel Billet
Cause Analysis on Surface Crack of Drill Steel 55SiMnMo Rolling Product and Process Improvement
Study and Application of a Casting Bloom Micro Segregation Model during Solidification Process of Bearing Steel GCrl5
Effect of Concasting Parameter and F-EMS on Center Carbon Segregation of 82B Steel Billet
Analysis on Surface Crack Formation Mechanism for Crankshaft Forgings of Steel 42CrMo and Process Improvement

Related Author

冯军
陈伟庆
朱叶
赵景存
安航航
张国锋
武佳毅
张龙

Related Institution

北京科技大学冶金与生态工程学院
(石钢京诚装备技术有限公司,)
宣化钢铁公司技术中心,宣化
四川建筑职业技术学院机电工程系
邯郸钢铁集团有限责任公司一炼钢厂
0